    PC flows at lower temp. Cures at higher temp. Try low temp for 5 min, then increase temp to cure.
    Whatever!

  2. #22
    Boolit Master murf205's Avatar
    Join Date
    Sep 2011
    Location
    Dead center of Alabama
    Posts
    2,410
    Quote Originally Posted by gnappi View Post
    Living in south Florida, humidity is very high in summer. Once I start, I'll tumble in the AC'd house, set them on trays, and bring them to the patio to bake. I'm hoping this works acceptably well, I have a LOT of projects lined up due to the post COVID crisis and pre-election buying frenzy.
    I think that storing AND tumbling in the AC is the best route in the more humid months. That has been my remedy since I started pc'ing. The 270 gr 44 boolits were done in July following that same procedure. Right now, in Alabama where I am, you can take a deep breath and get a minnow hung in your throat!! Yeah, that humid.Attachment 266969
    IT AINT what ya shoot--its how ya shoot it. NONE of us are as smart as ALL of us!

Page 2 of 2 FirstFirst 12

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check