When smelting down WW or Flashing or any other alloy what temp should be be smelting at for ignots . When I cast boolits in the lee pot that 675/725'F range works well for casting bullets
Is the same temp good for "smelting" in the big pot?
ex if Im blending 25lbs COWWS , 25lbs Flashing/soft , adding 2% tin should I be running the pot hotter to get the mix to alloy better or should I run closer to the "liquid" melt temp?