Hi guys, novice caster here, I came into aprox 250 lbs of water lead pipe that I have put into ingots, I have been casting for .44 mag and .357 from wheel weights and then powder coating,it has been working out pretty good. I realize #2 is harder than what i'm using but for my brain i'm using #2 for a starting point. I have tried to read as much as I can about making something a little softer than #2 I start to get confused when reading about different mixes so I was thinking about buying 5 lbs of antimony and 3 lbs of tin if my math is right if I mix 8oz 0f antimony and 8oz of tin per 20lbs of lead which is half of what #2 is would that give me closer to a 10 bnh? I'm trying to get as much mileage from my lead as possible for my needs. thanks in advance for any help.
Brian..