    New Lee 35 cal 200 gen 2 cavity

    Hello all, got a new Lee two cavity 35 cal 200 grn gc mold yesterday to try out in my 35 Whelan. I went out today and cleaned it up, heat cycled it a few times on top of my lead pot and smoked it with a bic. After the first few pours it started turning out some really nice looking boolits! They are cooling right now, so no word yet on weather or not they drop to size, but there are a pile of good looking boolits sitting on my bench waiting for pc and gas checks.
    Just figured on an update for new Lee mold.
    "Give me liberty, or give me death!" Patrick Henry ,March 23, 1775

  2. #2
    Banned

    tomme boy's Avatar
    Join Date
    May 2011
    Location
    Clinton, Iowa
    Posts
    5,200
    They are way better than the last couple versions they have had. If you did not know, the sprue plate bolt is a reverse thread.

  3. #3
    Boolit Buddy adcoch1's Avatar
    Join Date
    Oct 2016
    Location
    Centralia Wa
    Posts
    349
    Discovered the reverse thread spruce plate screw when adjusting plate tension. I had read that somewhere, so not a complete surprise. I am a newbie, but having great luck so far mostly...
    "Give me liberty, or give me death!" Patrick Henry ,March 23, 1775

  4. #4
    Boolit Master RU shooter's Avatar
    Join Date
    Nov 2006
    Location
    SW Pa.
    Posts
    2,928
    I got that mould when they first came out with it . Drops right at .359 with my alloy and at 205 grs shoots really well in my 35 Rem
    If you find yourself in a fair fight, your tactics suck!

  5. #5
    Boolit Master

    Join Date
    Feb 2012
    Location
    Foothills, NC
    Posts
    2,223
    Shoots well in my 358 Win. 1/12 twist.

  6. #6
    Boolit Master


    Bookworm's Avatar
    Join Date
    Jan 2016
    Location
    Central Oklahoma, on a dirt road.
    Posts
    1,186
    I got that mould to use in a H&R 357 single shot, as a 360DW.

    I cast some up, but haven't gotten around to working up a load.

  7. #7
    Boolit Buddy mike69's Avatar
    Join Date
    Jan 2016
    Location
    WV
    Posts
    154
    I'm having good luck with that mold in my Marlin 35 rem . Mine cast .358 with wheel weights .

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check