SPF to Kylongrifle32
The diameter of this mold is just a little too big at the bore-ride to chamber reliably in my gun after I powdercoat them. Boolits weigh in at 232 grains with my alloy. LOA measures at 1.367" on the sample. Diameter has a slight taper, from .314" at the rear to .301" at the front of the bore ride. (See the photos.) Of course, those dimensions are a little bigger with the PC, and the bolt on my AR can't always chamber the next round.
I will sell this mold for $55 shipped in a USPS Small Flat Rate Box to the first to post "I'll take it" in this thread. Please send a follow-up PM to exchange names and addresses. Payment by Cash, USPS Money Order, or your check is OK... Gotta wait for the check to clear, and no PayPal...
Attachment 247705 Attachment 247706 Attachment 247707
Attachment 247708 Attachment 247709
Driving band and Front band
Attachment 247710 Attachment 247711
Rear bore ride and Front bore ride