I have a alloy with 1.58% tin and 1.48% antimony.
I also have super hard 30% antimony, and stereo type available.
Ideally I would also like some arsenic for quench hardening.
How can I mix what I've got to get my desired 15-16bhn without the bullet becoming to hard.