New Lee 358-125-RF mold arrived today. I ordered it off eBay and got a good deal on it.
I decided to give it a try out this afternoon.
My pot is a Lee 4-20 and I got everything up to heat, lubed the mold and was dropping good boolits with the second cast.
The session went well. No problems with sticky boolits or wrinkles at all.
I ran it for 30 minutes and had 384 boolits on the table when I got done.
My alloy was range scrap so I am never certain until I get done what the boolits will weigh. These dropped at just under 130 grains.
They measure .359 right on the nose with my micrometer and they are ROUND. No mis-alignment or oval to them at all.
Lee was having a great day when they made this mold.
I will be able to use these in my 38/357 and my 9mm with no issues.
Now I need to get my lube sizer converted over to .357 and get some of these ready to go.