i have had scrap that was kept indoors for months that still ended up with condensation on it. are you putting everything in pot and heating or do you add after it is heated?
i have had scrap that was kept indoors for months that still ended up with condensation on it. are you putting everything in pot and heating or do you add after it is heated?
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |