I will start casting for my Makarov this Fall and I plan to pick up a flat point Noe mold for it. I will be using a flat point mold rather than a hollow point (unless anyone is interested in a group buy for such a thing) and the main intended use is target. However, I note that in this rather mild cartridge Lyman data suggests that lead boolits will move a lot faster than jacketed. For a self defense load, what alloy would I have to use to possibly get expansion/deformation at 1000 FPS? Pure? 16-1? Something else? Or is thus a fool's errand and such a thing should simply be counted on for penetration?