  1. #21
    Boolit Master FISH4BUGS's Avatar
    Join Date
    Jun 2005
    Location
    Inland from Seacoast New Hampshire
    Posts
    2,743
    Toothpaste it is. Now to just find the time to do 5 8 cavity H&G moulds! I'll just keep them well oiled and sealed in a Tupperware snap lid container until i can get to them.
    Collector and shooter of guns and other items that require a tax stamp, Lead and brass scrounger. Never too much brass, lead or components in inventory! Always looking to win beauty contests with my reloads.

  2. #22
    Boolit Master FISH4BUGS's Avatar
    Join Date
    Jun 2005
    Location
    Inland from Seacoast New Hampshire
    Posts
    2,743
    Actually I think i will use use Comet Cleanser. It is a mild abrasive and should work just fine. I will do one in Comet and the other in toothpaste.
    A bench report will come as soon as I get some time to do this.
    Collector and shooter of guns and other items that require a tax stamp, Lead and brass scrounger. Never too much brass, lead or components in inventory! Always looking to win beauty contests with my reloads.

  3. #23
    Boolit Master redhawk0's Avatar
    Join Date
    Apr 2016
    Location
    North East, USA
    Posts
    1,417
    Hahaha....Toothpaste to fix 8 cavities....You gotta love the irony.

    I've had good luck with JB Bore paste to just polish them up. Never tried toothpaste. Its now in my notes though.

    redhawk

    The only stupid question...is the unasked one.
    Not all who wander....are lost.
    "Common Sense" is like a flower. It doesn't grow in everyone's garden.

    If more government is the answer, then it was a really stupid question. - Ronald Reagan

  4. #24
    Boolit Master
    JBinMN's Avatar
    Join Date
    Feb 2017
    Location
    Goodhue County, SE Minnesota
    Posts
    3,080
    Not sure if you got to the molds yet, but In case you missed them, here are some of the "STICKY" topics at the top of this forum that describe the process you are, iof have been going to do... {Even though these are mostly for aluminum molds, they should help.)

    Maybe they will help if ya have not read them yet...

    Expanding a boolit mould the "WEET" method. (In parts)
    http://castboolits.gunloads.com/show...hod-(In-parts)

    Lee-menting: The Spinning of boolits
    http://castboolits.gunloads.com/show...ing-of-boolits

    Sure-Fire Lee-Menting Technique (Aimoo Post Revisited)
    http://castboolits.gunloads.com/show...ost-Revisited)

    Sticky: Lapping 301 -- Changing LEE feature diameters
    http://castboolits.gunloads.com/show...ture-diameters

    {I will also PM this post to ya , in case ya miss it here. }
    2nd Amend./U.S. Const. - "A well regulated Militia, being necessary to the security of a free State, the right of the people to keep and bear Arms, shall not be infringed."

    ~~ WWG1WGA ~~

    Restore the Republic!!!

    For the Fudds > "Those who appease a tiger, do so in the hope that the tiger will eat them last." -Winston Churchill.

    President Reagan tells it like it is: https://www.youtube.com/watch?v=c6MwPgPK7WQ

    Phil Robertson explains the Wall: https://youtu.be/f9d1Wof7S4o

Page 2 of 2 FirstFirst 12

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check