    copperrized lead ??

    A fellow caster stated that his lead has a lite copper haze floating on top ,," does he need to skim the copper haze off "??? Thought I would ask someone with knowledge of this subject ,,. Mentioned something about using copperized lead ???.




    coffee's ready,,,,Hootmix.

  2. #2
    Boolit Master
    lwknight's Avatar
    Join Date
    Nov 2009
    Location
    Fort Worth, Texas where the west begins
    Posts
    3,418
    That "light copper " haze sounds a whole lot what others call wheat straw color. Most likely it is from a high tin content. However some people purposely add a very small amount of copper to the alloy. Tin is required to dissolve the copper and what I read is that .5% is a lot. So there could very well be copper in the alloy and if it is then it probably has a goodly amount of tin as well.
    Anyway, no need to skim it off. It will just come right back and you are probably taking tin out in oxide form.
    Sent from my PC with a keyboard and camera on it with internet too.
    Melting Stuff is FUN!
    Shooting stuff is even funner

    L W Knight

  3. #3
    Boolit Master
    NoZombies's Avatar
    Join Date
    May 2009
    Location
    N. Florida
    Posts
    2,493
    It's most likely desirable elements separating due to excessive heat. The best thing he can do is flux the lead and try to mix everything back in, while lowering the heat a little bit.
    Nozombies.com Practical Zombie Survival

    Collecting .32 molds. Please let me know if you have one you don't need, cause I might "need" it!

  4. #4
    Boolit Grand Master

    Join Date
    Oct 2009
    Location
    England,Ar
    Posts
    7,693
    Another vote to not skim it off. I would try to stir and flux it back into the mix. Maybe reduce the melting temp a little.

  5. #5
    Boolit Master
    Join Date
    May 2014
    Posts
    1,439
    The yellow haze is lead sulfate. It used to be used as a dye in cloth mfg.
    QUIS CUSTODIET IPSOS CUSTODES?

  6. #6
    Boolit Buddy
    Join Date
    Nov 2017
    Location
    S.E. OKLA.
    Posts
    452
    Thank you I 'll pass this info along.

    coffee's ready,,,,Hootmix.

  7. #7
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    my first thought was tin, throw some sawdust in there and stir it good, maybe with a tidbit of beeswax, and it should go back into the mix.. I keep a layer of wood shavings ash on top of my melt, even in my bottom pour, to keep the tin from oxidizing, and it works great. I just never drain the pot completely, unless I have skimmed all that stuff off, very well. instead I usually leave maybe 2 lbs in it, and tip the machine so that the last bit of lead dries away from the valve and will come right out. that avoids sucking stuff through the valve, clogging it!
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check