  1. #21
    Boolit Master
    Join Date
    Nov 2005
    Location
    Bluegrass State
    Posts
    518
    I find 4 cavity brass too heavy. I like brass molds as I have several but limit them to 2 cavity. I only purchase iron or steel molds nowadays when they are vintage Lyman, RCBS, or my favorite iron mold, Saeco. If I need a 4 cavity mold, aluminum gets the nod. They all cast different depending on material, size of block, number of cavities and size of bullet. All will produce excellent bullets. I do preheat on a hot plate and usually keep the first bullet cast.

  2. #22
    Quote Originally Posted by gwpercle View Post
    I coat the inside and out, all parts with Liquid Wrench Dry Lubricant, it does not have to be removed , it acts as a release agent, it protects them from rust. And does not contaminate the cavities.
    Gary
    which one is it? i need to try it. the '''don't have to wipe it before use''' is interesting to me haha





  3. #23
    Boolit Master
    Ausglock's Avatar
    Join Date
    May 2010
    Location
    NSW North Coast, Australia
    Posts
    2,200
    Be aware that these type of products will prevent coatings from bonding to the bullets.
    HITEK coating will fail to stick. Most of these contain Silicone, and therein lies the problem.
    Hooroo.
    Regards, Trevor.
    Australia

  4. #24
    Quote Originally Posted by Ausglock View Post
    Be aware that these type of products will prevent coatings from bonding to the bullets.
    HITEK coating will fail to stick. Most of these contain Silicone, and therein lies the problem.
    i hadn't thought of that!!thanks for the reminder.

  5. #25
    Boolit Master
    Join Date
    May 2013
    Location
    Indianapolis, indiana
    Posts
    1,105
    my molds are made out of a 5 billion year old meteorite.

Page 2 of 2 FirstFirst 12

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check