Looking for some tips on powder. I have tite group, w231, vv320, universal clays, h110, blue dot, autocomp, wst, wsf, and be86.
Casting 356x120
401x175
358x158.
Powder coat and resized to 357, 401, 358.
Guns are glocks. Ar9 carbine. 586 and 686 with 6 inch barrels.
Testing some .40 with 4.0 of tg and 4.3 of w231.
Any guidance for the noob?
Thanks
Dino
sent from a tin can and a long string.