hello all my buy it now got the best of me and I got 10#s of pure antimony chunks and 10 #s of tin that will be here tomorrow shooting for a 90-5-5 alloy 100# batches whats the best approach to mixing it? slowly adding it to the mix or to melt the antimony first then add the lead and tin. I have read it will melt in slowly at a lower temp .its a pain .its easy but haven't found any step by step on the process besides what I have seen in the forums for fluxing I have lyman bullet lube and homemade bulletlube .sawdust and a lot of candle wax if it will help it I can through in the wifes cats and dogs in if it will speed up the process any tips and tricks are appreciated just playing on the cats and dogs im saving them for the zombie apocalypse