Well this has been an interesting season for me. The start up I was working for ran out of money early in Dec. so, using the time I have, I've spent the past couple of weeks casting boolits! So far 1500 9mm 125gr rn from a 6 cavity Lee mould..
Interestingly enough, it took the first 1000 to break in the mould, then after that it was dropping perfect boolits! Now I have to make up some more alloy (5% antimony, 1% tin) and crank out another 3000 or so to keep from running dry this spring/summer!
So, Merry Christmas to all (even the Hanukkah folk) especially those that have taken the time to answer my questions!