  1. #2761
    Boolit Master freebullet's Avatar
    Join Date
    Mar 2013
    Location
    Nebraska
    Posts
    1,473
    What did you use to recover those?
    If you think your a hammer everything looks like a nail.

  2. #2762
    Love Life
    Guest
    Interesting indeed. Hmmm...

    I almost want to put up another drawing board, but I just want to get blasting!!

    You can tell which bullets are Glock fired.

    I have more bullets floating around fired from various other Glocks that appear the same as the Glock shot bullets here. You can see the coating stripping at the rifling edge of the traditional rifled barrels. I've never experienced any leading though.
    Last edited by Love Life; 04-07-2014 at 12:22 AM.

  3. #2763
    Boolit Master




    HI-TEK's Avatar
    Join Date
    Aug 2012
    Location
    Australia
    Posts
    2,162
    Quote Originally Posted by Love Life View Post
    Interesting indeed. Hmmm...

    I almost want to put up another drawing board, but I just want to get blasting!!

    You can tell which bullets are Glock fired.

    I have more bullets floating around fired from various other Glocks that appear the same as the Glock shot bullets here. You can see the coating stripping at the rifling edge. I've never experienced any leading though.
    Congratulations on your reaching 10,000 blogs.
    Well done

  4. #2764
    Love Life
    Guest
    Holy smokes. I really need to get a life...

  5. #2765
    Boolit Master freebullet's Avatar
    Join Date
    Mar 2013
    Location
    Nebraska
    Posts
    1,473
    I'm curious on average how many beautiful women give you their # if firing hitek from glocks?
    If you think your a hammer everything looks like a nail.

  6. #2766
    Love Life
    Guest
    Pretty bullets plus a ninja gun? Hot women get in fist fights just for the opportunity to give me gas money.

  7. #2767
    Boolit Master freebullet's Avatar
    Join Date
    Mar 2013
    Location
    Nebraska
    Posts
    1,473
    Lol, I didn't think you'd pass on a setup like that lol.
    If you think your a hammer everything looks like a nail.

  8. #2768
    Boolit Grand Master
    btroj's Avatar
    Join Date
    May 2006
    Location
    Nebraska's oldest city
    Posts
    12,418
    Quote Originally Posted by freebullet View Post
    What did you use to recover those?
    The berm. First pistol bay on left as you pull in. Right by the ports potties.
    You will learn far more at the casting, loading, and shooting bench than you ever will at a computer bench.

  9. #2769
    Boolit Buddy
    Join Date
    Oct 2013
    Location
    Pensacola, Fla
    Posts
    232
    Quote Originally Posted by Love Life View Post
    Interesting indeed. Hmmm...

    I almost want to put up another drawing board, but I just want to get blasting!!

    You can tell which bullets are Glock fired.

    I have more bullets floating around fired from various other Glocks that appear the same as the Glock shot bullets here. You can see the coating stripping at the rifling edge of the traditional rifled barrels. I've never experienced any leading though.
    these are how mine look also. i dont have a glock but all my blackhawks and my 70 series colt 1911 cut the coating at the edge. i dont get leading unless im running loads that are too hot for a non gaschecked boolit. ive got a gascheck .44 mold on the way so ill see how that does.

  10. #2770
    Boolit Master

    Join Date
    Sep 2011
    Location
    Northeast Ohio
    Posts
    923
    I just ordered a 4 cavity 9 MM 115 grain RN Iron Mold

    and a 45 cal 4 cavity 230 grain RN Iron Mold, both have 3 locating pins.

    MOLDS ARE SMOOTH, NO LUBE GROOVES.

    Hardline Industries has them on E-Bay for 1 day at $125 each, plus shipping (BUY NOW) price.

  11. #2771
    Boolit Master

    Join Date
    Sep 2011
    Location
    Northeast Ohio
    Posts
    923
    Just got a message from Mike at Hardline Industries, my NEW 9 MM & 45 cal

    NO LUBE GROOVE 4 cavity Iron molds I ordered during the nighttime

    from E-Bay ($125 each + ship) will ship out today.

    Nice work MIKE & DERRICK at Hardline Industries.

    I like the 3 alignment pin deal.

    GOOD reviews from Love Life and gunoil here on the Forum for these molds.

    I need to work up some alloy.

    Can't hardly wait for the NEW Dry Powder HI-TEK stuff to reach the USA.

  12. #2772
    Boolit Master




    HI-TEK's Avatar
    Join Date
    Aug 2012
    Location
    Australia
    Posts
    2,162
    Quote Originally Posted by Moonman View Post
    Just got a message from Mike at Hardline Industries, my NEW 9 MM & 45 cal

    NO LUBE GROOVE 4 cavity Iron molds I ordered during the nighttime

    from E-Bay ($125 each + ship) will ship out today.

    Nice work MIKE & DERRICK at Hardline Industries.

    I like the 3 alignment pin deal.

    GOOD reviews from Love Life and gunoil here on the Forum for these molds.

    I need to work up some alloy.

    Can't hardly wait for the NEW Dry Powder HI-TEK stuff to reach the USA.
    Just a quick update.
    Made some powdered product, which will be sent to US when local testing has confirmed test is OK.
    Will keep you posted.
    Commercial production and availability is 6-8 weeks away.
    Orders for commercial quantities are pending.
    So far, all looks great.
    Thanks much for your interest.

  13. #2773
    Boolit Master
    Ausglock's Avatar
    Join Date
    May 2010
    Location
    NSW North Coast, Australia
    Posts
    3,163
    Woohoo. More DRI_TEK Supercoat samples to play with.
    Hooroo.
    Regards, Trevor.
    Australia

  14. #2774
    Boolit Master

    Join Date
    Sep 2011
    Location
    Northeast Ohio
    Posts
    923
    Ausglock,

    Get to testing the stuff so HI-TEK Joe knows when he can start shipping the DRY to the USA.

    Moonman

  15. #2775
    Boolit Master

    Join Date
    Sep 2011
    Location
    Northeast Ohio
    Posts
    923
    Donnie at Bayou Bullets E-Mailed me about the Aerosol HI-TEK Mold Release,

    he's waiting on labels, said it should be available in about another week.

    MOONMAN

  16. #2776
    Boolit Buddy
    Join Date
    Feb 2012
    Posts
    279
    Hope we have some Kryptonite Green in the dry powders coming stateside in the near future.

  17. #2777
    Boolit Master
    Ausglock's Avatar
    Join Date
    May 2010
    Location
    NSW North Coast, Australia
    Posts
    3,163
    Kryptonite green can' t be powdered. Zombie green can.
    Hooroo.
    Regards, Trevor.
    Australia

  18. #2778
    Boolit Master

    Join Date
    Sep 2011
    Location
    Northeast Ohio
    Posts
    923
    Trevor,

    Do you have photos of Zombie and Kryptonite Green pills to show color difference?

  19. #2779
    Boolit Master




    HI-TEK's Avatar
    Join Date
    Aug 2012
    Location
    Australia
    Posts
    2,162
    Quote Originally Posted by Moonman View Post
    Trevor,

    Do you have photos of Zombie and Kryptonite Green pills to show color difference?
    Attached are Zombie & Kryptonite green photos.Click image for larger version. 

Name:	Kryptonite Green.jpg 
Views:	115 
Size:	56.6 KB 
ID:	101815Click image for larger version. 

Name:	Zombie424.jpg 
Views:	129 
Size:	88.2 KB 
ID:	101816

  20. #2780
    Boolit Master
    Ausglock's Avatar
    Join Date
    May 2010
    Location
    NSW North Coast, Australia
    Posts
    3,163
    The zombie is a bit lighter green than the photo shows.
    Hooroo.
    Regards, Trevor.
    Australia

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check