Here are the results of my latest experiment. They actually turned out rather well.
And some 160 grain for my Mosin
Here are the results of my latest experiment. They actually turned out rather well.
And some 160 grain for my Mosin
Ok, they look pretty good, how did you plate them?
- MikeS
Want to checkout my feedback? It's here:
http://www.castboolits.gunloads.com/...d.php?t=136410
I fooled with plating, then found that proper boolit fit and a good lube was much easier, but I have to say those look pretty good.
How do they shoot and how's the bore for residue after, say, thirty rounds?
this is awesome to look at but we need details please
Ray
I can plate copper onto lead! But mercy, after I scaled it up to do 20 at a time and after a month of tinkering, mine were still awful. I gave it up. Very pretty rounds. Wish I coulda made it work.
War is peace.
Freedom is slavery.
Ignorance is strength.”
― George Orwell, 1984
Try tumbling them with steel BBs. Makes em purdy!
Really Pretty! Got a bunch of chems sitting around, just to try that very thing, when I get the time. Really nice!!
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |