I just took an order for 1K boolits.
I have ~ 50 in the box.
So, I fired up the melter and went to work.
Last time (about 2 weeks ago) I used this mold I got 99% good from it.
Today, I got 99% rejects.
Same alloy, same temps (mold is instrumented), same fluxing.
Every thing was the same. I even sat in the same chair
I couldn't pour a usable boolit to save my ****!
SIGH