    Lead pipe can give you some funny stuff.
    Click image for larger version. 

Name:	mystery metal.jpg 
Views:	26 
Size:	61.1 KB 
ID:	202034

  2. #222
    Boolit Grand Master Good Cheer's Avatar
    Join Date
    Jul 2010
    Location
    the Ark
    Posts
    5,276
    So far my copper experience is pretty limited, just working with a couple of spools of #2 babbitt wire. Still learning and will enjoy reading back through the thread. Thanks to all.

  3. #223
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    good cheer, just what the heck is that?
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

  4. #224
    Banned

    Join Date
    Dec 2007
    Location
    soda springs Id.
    Posts
    28,088
    calcium.

  5. #225
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    oh, duh... now that you point it out to me, it should have been obvious, but I've never heard of it recrystallizing like that. interesting
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

  6. #226
    Banned

    Join Date
    Dec 2007
    Location
    soda springs Id.
    Posts
    28,088
    oh yeah, you should see inside my water heater.
    bonus is my pipes never leak.

  7. #227
    Boolit Buddy
    Join Date
    Jan 2015
    Location
    Reno, NV
    Posts
    109
    I've been through both of these threads on Cu alloys and had a thought.

    Could you take soft lead, add brass case trimming shavings, remove the zinc, then add linotype? It would solve a number of issues, with Sn not being removed from the alloy with the Zn, and still add Sb and Sn in a known alloy that adds hardness with the Cu/Pb?

    I realize this is a gross simplification, but seems to solve most of the issues. The only open question would be ratios.......

  8. #228
    Banned

    Join Date
    Dec 2007
    Location
    soda springs Id.
    Posts
    28,088
    I ain't tried brass [thought about it]
    but initial testing was done with a higher tin solution alloy and tinned speaker wire cut into small pieces.

  9. #229
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    the problem would be the high melting point of brass I think, even copper wont mix unless it is tinned or it iss in the form of copper sulfide, like Zepps is
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

  10. #230
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    I have noticed that copper laced boolits have a harder, slicker "skin" to them, even if the BHN itself isn't very high, mine are around 13.5 for example. has anyone else noticed this? and do you think that it helps with ballistics, wether it be pressure-wise or accuracy?
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

  11. #231
    Boolit Buddy
    Join Date
    Jan 2015
    Location
    Reno, NV
    Posts
    109
    Someone on one of these threads added brass case trimmings and said they were successful.

    I'm looking for cheap, easy, and successful.

  12. #232
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    a 2lb bottle of Zepps is only like 11.99-12.99 at home depo, aand that goes a long way. it is 25% copper, so you can figure out easily how much you want/ need in relation to the zinc and what you want your finished cu % to be
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

  13. #233
    Boolit Master
    Chev. William's Avatar
    Join Date
    Aug 2013
    Location
    Sun Valley, California
    Posts
    1,956
    NOTE: Eutectic Lead-Tin Solder at ~63% Tin Will Disolve some Copper at SOLDERING temperatures. In Electronics Industry we went to a Semi eutectic Alloy Containing Silver to stop the removal of Copper Fine Line Traces on Modern Design Circuit Boards.

    Best Regards,
    Chev. William

  14. #234
    Boolit Master Oklahoma Rebel's Avatar
    Join Date
    Nov 2015
    Location
    outside of Sand Springs, N.E. OK
    Posts
    2,353
    so, for a 3sb/3sn/.25-.35%cu alloy, what do you think would be the best choice for hollowpoint pins, short and fat, long and skinny, or other? I was thinking a hp shaped like a martini glass would work good ( short sect. of wide opening, then a longer "stem" of maybe .10 dia ending in a rounded point), if you can picture what I mean? and do you think this alloy should be heat treated or quenched for 2100fps?
    An armed man in a citizen.
    An unarmed man is a subject.
    A disarmed man is a slave.

Page 12 of 12 FirstFirst ... 23456789101112

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check