Cast up some 50 / 50 with 1% tin, after 2 days ageing it reads 7.9 bhn. I dont know if this is hard enough with .454, 263gr. boolits. Two holes a must evry time.
Cast up some 50 / 50 with 1% tin, after 2 days ageing it reads 7.9 bhn. I dont know if this is hard enough with .454, 263gr. boolits. Two holes a must evry time.
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |