    Quote Originally Posted by Springfield View Post
    You guys just need more ingot moulds! I like to do 50 lbs at a time, then while the new batch is melting the ingots cool off enough.
    Only 50# at a time, I do 125# at a time and do the same, Empty molds, just before I am ready to repour.

    Sam
    Muddy Creek Sam
    |__
    ( o )\_
    USN 100% Disabled
    Dark Lord of The Soot
    SBSS# 2137
    LASSOOS#1957s
    SASS VET #131
    http://www.muddycreeksam.com


    My Feedback!
    http://castboolits.gunloads.com/showthread.php?t=66946

  2. #22
    Boolit Master


    GT27's Avatar
    Join Date
    Nov 2009
    Location
    NEPA
    Posts
    603
    Quote Originally Posted by slabbandit View Post
    Sounds like I'm getting my lead and my Lee mold pans too hot!
    Bingo,we have a winner!!!
    You can't buy common sense,and stupidity can't be fixed!

  3. #23
    Boolit Master
    lwknight's Avatar
    Join Date
    Nov 2009
    Location
    Fort Worth, Texas where the west begins
    Posts
    3,418
    Wait till you try linotype.
    It looks hard and solid till you dump it.
    It will be still water thin liquid in the middle.
    Sent from my PC with a keyboard and camera on it with internet too.
    Melting Stuff is FUN!
    Shooting stuff is even funner

    L W Knight

  4. #24
    Boolit Master
    Dennis Eugene's Avatar
    Join Date
    Mar 2007
    Location
    Craig, Prince of Wales Island, Alaska
    Posts
    875
    If you set you ingot molds down in the snow they cool off much faster that's what I do. Dennis

  5. #25
    Banned


    Join Date
    Mar 2009
    Location
    29˚68’27”N, 99˚12’07”W
    Posts
    14,662
    Dennis, you keep talking about this think called "snow" on the forum, even posted a few pics of what it looks like, but I still don't know what the heck you're talking about!

    Gear

  6. #26
    Boolit Grand Master

    mold maker's Avatar
    Join Date
    Jul 2007
    Location
    Piedmont (Conover) NC
    Posts
    5,429
    If I had to wait on snow, I'd only get to smelt once or twice, in 5 years. I have invested in multiple molds of each type. I use a different type, for each kind of lead. In all I have 5-7 each of 6 kinds of ingot mold. I can always get most of my money back selling them.
    Plus I'm too old to worry about speed. I'm never going to finish the bucket list, so why hurry/worry?

Page 2 of 2 FirstFirst 12

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check