    I bought sheet lead and plumbing pipe from a...

    I bought sheet lead and plumbing pipe from a scrap yard for $.75 a pound. 3 to 400 lbs. The nice thing was that they sheared it into managable pieces for me at no extra cost. A few days before I...
  2. Replies
    23
    Views
    3,482

    Forum: Cast Boolits

    Way to go! Now you have a place to spend your...

    Way to go! Now you have a place to spend your mad money.
  3. Thread: 9mm problem

    by duxnbux
    Replies
    4
    Views
    1,142

    Forum: Cast Boolits

    More info on 9mm. I'm casting tumble lube...

    More info on 9mm. I'm casting tumble lube boolits hoping to be able to skip sizing.
  4. Thread: 9mm problem

    by duxnbux
    Replies
    4
    Views
    1,142

    Forum: Cast Boolits

    9mm problem

    I want to load my 9mm boolits which are 124 gr truncated cone. Lee 90402 six banger. I'm using Richard Lee's Modern Reloading charts and it calls for a start of 5.3 Unique. I'm using Uniquersky...
  5. Replies
    0
    Views
    910

    Forum: Cast Boolits

    My first sawdust flux job

    I stopped by Home Depot and got a bag of sawdust to use as flux since you guys reccommend it so highly. Boy, it works slick as a gut!

    I don't have to be concerned about wasting flux now.

    I...
  6. Thread: Age hardening

    by duxnbux
    Replies
    15
    Views
    3,636

    Forum: Cast Boolits

    Thanks Rick I'm using a Lee bhn tester. Like...

    Thanks Rick
    I'm using a Lee bhn tester. Like others have said, it's tricky to get used to but seems to work well after the learning curve has been completed.
    Your info was very helpful regarding...
  7. Thread: Age hardening

    by duxnbux
    Replies
    15
    Views
    3,636

    Forum: Cast Boolits

    Age hardening

    I'm new to the forum, been lurking for a few weeks and am impressed with the knowledge I've seen here.
    I am smelting 50/50 lino and lead. #2? It tests about 15 bhn after a few days. When I cast it...
  8. Replies
    817
    Views
    623,982

    Forum: Cast Boolits

    Sticky: Hello to a bunch of sharp, courteous dudes- and...

    Hello to a bunch of sharp, courteous dudes- and dudettes, I assume.

    I've been lurking for a few weeks and am impressed with the amount of knowledge you folks share with others.
    I've been...
Results 1 to 8 of 8
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check