Hi, I have finished up smelting all my COWW into ingots (boy that was a major job). I hand sorted all the COWW while using sidecutter dike. All total I only had 4 zinc & 2 steel floaters. Kept the melting temp to 670 to 690 degrees. Fluxed with sawdust & wax. Numerous fluxing, all cleaned up very well. I just finished today the 1st load of SOWW. I still have 2 more loads to smelt of SOWW.
I will be re-smelting the COWW (50 lbs of it) taking x amt of ingots from 10 lots that was done to uniform that amount. Then I intend to put in 50 Ibs of SOWW plus 2% pewter.
I can repeat this action as more is needed later. At least I wll have some to use for making boolits.
We have a 1- 380acp, 2- 9mm acps, 1-38 spl revolver, 1- 357 mag (sp101), 1-45acp & 2- 30-30's.
So my question is - will the above mix (50-50-2%) work for the above weapons? If not, I am certainly open to suggestions and any help or guidence in this matter.
TYVM in advance,
SharuLady