Yeah, but the misinformation hasn't changed a bit! [smilie=b:
Jerry
03-27-2016, 12:19 AM
Ural Driver
Thanks for reminding me. :idea: I just ordered another 50# from Rotometals. :cbpour:
03-27-2016, 08:23 AM
44man
Quote:
Originally Posted by fredj338
I will only add that trying to blend oure antimony w/ your alloy is going to eb diff as the melting temp is so high. Better to use an alloy w/ antimony in it, like lead shot or ww, then add tin to that.
Antimony melts in at 600° with a proper flux.
I never fooled with no. 2, too much tin and cost with little benefit.