Just a quick footnote, when you are ordering plain hard cast product, please ask your supplier if he uses any release agent in his casting moulds.
Sometimes, (if used), these type of release agents, will also later interfere with coating bonding to alloy.
What is needed with casting, is a non "wet" type of release agent, that will not transfer to alloy, but release projectile cleanly from moulds.
If you have a talk with Donnie, at Bayou, he can make recommendations about such material.
Your caster may also talk with Donnie about a product called Hi-Tek 500 Plus.
Many, including home casters have found great results with clean release and no problems with coating afterwards.
Hope this helps.