Originally Posted by
tazman
Got in a lyman 358311 I purchased off eBay today. I heated up the Lee 4-20, got the mold up to heat, and had at it.
Things went really well. In about 90 minutes I had just over 500 boolits on the table. The mold was a 2 cavity and dropped easily and cleanly.
With my alloy the boolits were coming out at 165 grains and .3575-.358 diameter. Since I tumble lube, I don't even need to run them through sizer.
Tomorrow after they have dried I will load some and go to the range.