So did my first legit casting session today.
Alloy was 100% clip on wheel weights
Pot temp ranged from 750 on the low side to 950 on the high side.
Mold was a Lee 225-55gr six cavity
Boolits where water dropped
Out side temp was around 50
Attachment 274710
Attachment 274711Attachment 274712Attachment 274713
They all look pretty decent to me this being the worst ok one out the bunch. Definetly pitching this one
Attachment 274714
But what do y'all think ? I'm powder coating and gas checking these as well