While smelting some lead belts i thoughtvof using pork fat as a flux. I used 1lb to 150 lbs of lead. Pritty smokey but most of the oxide went back to metal plus the garrage now smells of baccon. The fat bubbled for a while then turned to ash. I scooped off the ash and what draus was there was. Would any other animal fat produce good results? Has anyone tried this and dose this work on the same princible as using saw dust?