    When in a .45 mood. I have two- six cavity lee molds. Rotating between them I can run as fast as I can keep lead melted. I have a couple NOE molds for the good stuff, but for smashing plates the lee molds are just fine.
    18 replies | 537 view(s)
  • Smk SHoe's Avatar
    01-03-2018, 07:31 PM
    A lot of people here don't gas check until the velocities get up. I load a lot for a .223 AR and don't gas check them. I haven't had any problems. You active now? and what Piece you on ( FA)
    19 replies | 1797 view(s)
No More Results
About Smk SHoe

Basic Information

About Smk SHoe
Biography:
Retired Regleg, Reloaded for 105, 155, and 203mm cannons
Location:
Sanford, NC
Interests:
Benchrest shooting
Occupation:
Driving Skateboards

Signature


Retired Redleg
I came into this world kicking and screaming covered in someone else's blood, I don't mind going out the same way.

Statistics


Total Posts
Total Posts
291
Posts Per Day
0.39
General Information
Last Activity
Yesterday 11:14 PM
Join Date
01-01-2016
Referrals
0
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check