  • sunburn's Avatar
    10-16-2017, 07:05 PM
    I appreciate booolits can be coated as soon as room temp and dry, sorry, let me be specific this time. Is there any advantage to letting the lead cure weeks or months before coating? Not looking for a specific BHN, just to improve on an existing...
    171 replies | 37618 view(s)
  • sunburn's Avatar
    10-15-2017, 03:34 PM
    How long should you wait after casting to coat the Boolits? Also, as I water drop from the mold after casting, is there any advantage of water dropping after the 2nd coat? Thanks for the Hi-Tek products, they make casting worthwhile.
    171 replies | 37618 view(s)
No More Results
About sunburn

Basic Information

Signature


For some reason, Islamists are the only racist, sexist, homophobic theocrats the media can't summon outrage against.

Statistics


Total Posts
Total Posts
35
Posts Per Day
0.02
General Information
Last Activity
10-17-2017 06:17 AM
Join Date
05-14-2013
Referrals
0
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check