    02-12-2018, 09:32 PM
    doghunter replied to a thread Question on alloys in Cast Boolits
    I'll try adding 50% stick on WW lead. Thanks for the suggestion.
    11 replies | 273 view(s)
  • doghunter's Avatar
    02-12-2018, 04:15 PM
    I was loading buckshot in a capsule in a 38 special for a while. 3 #1 buck would just fit in a speer capsule. They would hold a palm sized pattern at 5-7 yards. the problem I had was that the buckshot would bust the capsule during recoil. I tried...
    17 replies | 1811 view(s)
  • doghunter's Avatar
    02-12-2018, 04:02 PM
    doghunter replied to a thread Question on alloys in Cast Boolits
    Thanks, I will try powder coating. I'm not really worried about exact sizes as long as they shoot ok. I just thought that because they were both undersized by about .005, that it might be something I was doing wrong. I originally got on here to...
    11 replies | 273 view(s)
  • doghunter's Avatar
    02-12-2018, 03:57 PM
    doghunter replied to a thread Question on alloys in Cast Boolits
    Thank you for the offer. I have some red powder from HF and plan to order some better stuff when I get around to it.
    11 replies | 273 view(s)
  • doghunter's Avatar
    02-12-2018, 08:15 AM
    That's the only thing Barack Obama ever did for me. Got me trying to be as self sufficient as I can in the ammunition dept.
    91 replies | 1991 view(s)
  • doghunter's Avatar
    02-12-2018, 07:53 AM
    doghunter replied to a thread Question on alloys in Cast Boolits
    I'm waiting on more hulls then I will try them like they are. I have a good load worked up with a 33 cal 54 gr pellet. As for the buck, they will probably work. Might even be able to add 2 more pellets to the load. Not sure how a .4005 bullet...
    11 replies | 273 view(s)
  • doghunter's Avatar
    02-12-2018, 06:51 AM
    I posted this in the alloys section, but didn't get any response, so please forgive the double post. Just finished my first casting session. The 2 molds I have are a Lee 18 Cavity 00 buckshot mold, and a Lee 6 cavity .401 175 gr flat point mold....
    11 replies | 273 view(s)
  • doghunter's Avatar
    02-10-2018, 05:35 PM
    Just finished my first casting session. The 2 molds I have are a Lee 18 Cavity 00 buckshot mold, and a Lee 6 cavity .401 175 gr flat point mold. My plan was to put 10 pounds of clip on wheel weight ingots in the pot and add 2% tin. That was a lot...
    0 replies | 100 view(s)
No More Results
About doghunter

Basic Information

Statistics


Total Posts
Total Posts
11
Posts Per Day
0.00
General Information
Last Activity
Yesterday 10:41 PM
Join Date
08-12-2009
Referrals
0
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check