Third casting session went better. Probably about 30% rejects. Considering the MiHec was brand new I dont think that is bad.

300 blackout is a NOE .311 230 grain Flat nose. A fellow forum member yondering removed the lube groves. It now drops around 244 grains.

9mm is a MiHec .359-125grain (9mm) HP Flat base.


http://i66.tinypic.com/1jrqq8.jpg

gwpercle
10-15-2016, 07:16 PM
Doing good...third time's the charm.

Actually moulds , especially aluminum and brass , need to be broken in, the cavities will develop a coating only achieved by casting. Mine start acting right after three heat cycling sessions ( no casting just heating and let slowly cool ) and then after the third casting session, they are good to go.
Gary

aaholland
10-16-2016, 04:17 PM
Powder coated today.

http://i67.tinypic.com/bi9uhh.jpg

WFO2
10-16-2016, 11:08 PM
Nice work .

bigolsmokebomb
10-17-2016, 10:06 PM
those look good. your PC job looks a lot better than mine but it may be the powder you're using too. all ive got is the good ol HF red

aaholland
10-18-2016, 05:38 AM
Its smokes powder. A guy from this form. I actually do two thin coats. With the 300 blackout i actually rub off the powder off the top of the bullet so the driving area is only thickly covered.

Boolseye
10-19-2016, 08:45 PM
Pretty molds.