PDA

View Full Version : range leqad / ww's



quiknot
01-28-2007, 02:00 PM
i am able to collect lead from and indoor range that I smelt down to use in casting my boolits....

question is (maybe it has been covered) is: do I need to add any ww's to it or is it good to go as is?

I shoot a 45LC with light loads, 230gr boolit

thanks

ron brooks
01-28-2007, 02:05 PM
For light loads you should be fine. This is assuming that the boolits are of the proper size.

Good luck,

Ron

mag_01
01-28-2007, 04:21 PM
Those range scraps will be go to go with what you are doing---Mag

imashooter2
01-28-2007, 04:54 PM
The same question was asked few days ago:

http://castboolits.gunloads.com/showthread.php?t=12614

As I said in that thread, the scrap I get from an indoor range is probably 50% .22's, 25% jacketed and 25% commercial cast. It casts beautifully as is and when quenched from the mold, it hardens up just like WW (to my very unscientific scratch tests).

I just spent a couple hours in the shed with that alloy this morning and have another 32 pounds of Lee 452-228-1R to add to my stash.