PDA

View Full Version : Reheating heat treated boolits



fecmech
02-11-2011, 04:34 PM
Can anyone tell me if I reheat some heat treated boolits to say 130-150 deg F to apply "Recluse" lube (45-45-10) if it will affect the original HT in any way?? Thanks Nick

felix
02-11-2011, 04:36 PM
No problem, Nick. It takes at least 250F to begin any anneal for anything metallic. ... felix

fecmech
02-11-2011, 07:02 PM
Thanks Felix

Fire_stick
02-12-2011, 02:46 AM
Good question. I was wonder the same thing today.

So if I have some heat treated bullets, and I want to make them soft again, I just heat them up to around 250 for a time then let them slow cool. Right? Or would the magic number be a little higher?

Gohon
02-12-2011, 11:39 AM
I would heat them at 350-400 degrees for an hour and let them air cool which would return them to the hardness they would have been if air cooled from the mold. Least ways that's how I've done it with success.

Dannix
02-12-2011, 01:07 PM
I've never heard of heating boolits to apply lube. I need to do some reading.

Informative post. Thanks felix.